Sample Fabrication

Substrate

...

  • 6/11/2012         Laser cut into 7x7 mm sample, solvent clean
    Debris due to laser cut observed
    On 6/13/2012, found out that this laser cutting procedure raises a normal silicon sample temperature high enough to hard-bake the photoresist, so it could have initiated gold diffusion on 4b.
Sample 4C
  • 6/5/2012           Raman measurements
  •