- 6/14/2012 SEM and EBSD. No evidence of breakdown or faulting. EBSD shows good (100) oriented single-crystal throughout.
Spot 2b tilt 2.tif
Spot 2b 90kx.tif
Spot 2b 300kx.tif
Spot 2b failed fib crater.tif
- 6/15/2012 TEM. FIB sample is unpolished at present, so visible amorphized regions are present on faces of coupon. Nevertheless, sample is single-crystalline and free of stacking faults and cellular breakdown.
Lowmag offaxis 8.jpg
Very low mag.jpg
Lowmag offaxis 6.jpg
Highmag offaxis 3.jpg
FFT of Highmag offaxis 3.jpg
Highmag offaxis 4.jpg
FFT of Highmag offaxis 4.jpg
Highmag offaxis 5.jpg
FFT of Highmag offaxis 5.jpg
Highmag offaxis 6.jpg
FFT of Highmag offaxis 6.jpg
Highmag offaxis 8.jpg
FFT of Highmag offaxis 8.jpg