6/11/2012         Laser cut into 7x7 mm sample, solvent clean
Debris due to laser cut observed
On 6/13/2012, found out that this laser cutting procedure raises a normal silicon sample temperature high enough to hard-bake the photoresist, so it can possibly initiate could have initiated gold diffusion on 4a.

Sample 4b
6/11/2012         Laser cut into 7x7 mm sample, solvent clean
Debris due to laser cut observed
On 6/13/2012, found out that this laser cutting procedure raises a normal silicon sample temperature high enough to hard-bake the photoresist, so it can possibly initiate gold diffusion so it could have initiated gold diffusion on 4b.