- 6/4/2012 UV-VIS reflection measurement
20120604 UV-VIS reflection Au 1a.Sample.Raw.csv
- 6/5/2012 UV-VIS transmission measurement
20120605 UV-VIS transmission Au 1a.Sample.Raw.csv
- 6/13/2012 Spin photoresist and bake at 115 C for 1 minute to protect sample from debris during laser cut
- 7/10/2012 Retook UV-VIS after tool lamp change
20120709 Au UV-VIS.xlsx
Sample 1B
- 6/13/2012 Spin photoresist and bake at 115 C for 1 minute to protect sample from debris during laser cut
...