6/5/2012 UV-VIS transmission measurement
20120605 UV-VIS transmission Au 1a.Sample.Raw.csv
6/1113/2012 Laser cut into 7x7 mm sample, solvent cleanSample 1b Spin photoresist and bake at 115 C for 1 minute to protect sample from debris during laser cut
Sample 2b
6/1113/2012 Laser cut into 7x7 mm sample, solvent clean Spin photoresist and bake at 115 C for 1 minute to protect sample from debris during laser cut