5-Layer Fiberglass | 10-Layer Fiberglass | |
---|---|---|
Control (West Systems epoxy) | ||
West Systems + Phenolic microballoons | ||
West Systems + Cork microballoons | ||
West Systems + High temperature paint | ||
West Systems + Cotronics 4700 |
Sample Preparation:
- Used West Systems epoxy to make 4 of 8" x 8" sheets of fiberglass (2 x 5 layers, 2 x 10 layers)
- Sand with a Dremel, then with 400-grit sandpaper. Make sure to sand the shiny side
- Mark and cut into 1.5" x 1.5" squares.
- Record mass of each sample.
Below is the test matrix for the parameters measured during this test. (Fill later with results).
...